文章摘要
Ti-48Al-2Nb-2Cr合金铸造收缩特性研究
Contraction Characteristics of Ti-48Al-2Nb-2Cr Casting Alloy
Received:April 08, 2018  Revised:May 10, 2018
DOI:10.3969/j.issn.1674-6457.2018.03.004
中文关键词: TiAl合金  熔模铸造  收缩率
英文关键词: TiAl alloy  investment casting  contraction rate
基金项目:装备预研基金(6140922020107);国家自然科学基金(51671026)
Author NameAffiliation
WEI Zhan-lei 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
REN Gui-juan Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China 
LI Jian-chong 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
HUANG Dong 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
MO Xiao-fei 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
LUO Qian 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
NAN Hai 1. AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China
2. Beijing Engineering Research Center of Advanced Titanium Alloy Precision Forming Technology, Beijing 100095, China 
Hits: 4588
Download times: 3971
中文摘要:
      目的 研究TiAl合金铸造过程的收缩特性。方法 采用Ti4822合金,通过设计长方体、圆柱体、回字形和环形4种典型结构,开展了熔模精密铸造工艺实验。结果 基础尺寸在10~80 mm时,Ti4822合金的自由线收缩率在3.11%~2.09%之间,受阻收缩比自由收缩低30%~50%左右,同时随着基础尺寸的增加,自由线收缩量增加,而收缩率呈降低趋势。结论 收缩数据和规律的获得,为TiAl合金铸件尺寸精度控制提供了基础数据。
英文摘要:
      In order to investigate the contraction characteristics of TiAl alloy,four kinds of typical structure were designed to carry out an experiment on investment casting process of Ti4822 alloy. The result showed that the free linear contraction rate of Ti4822 alloy was 3.11% to 2.09% when the basic dimension was 10~80 mm. Furthermore, the hindered linear contraction rate was 30%~50% lower than the free linear contraction rate. Besides, the contraction quantity increased with the improvement of basic dimension, while the contraction rate declined. The acquiring of contraction characteristics and rules provides basic data for controlling the dimension accuracy of TiAl alloy casting.
View Full Text   View/Add Comment  Download reader
Close

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

You are the551889visitor    渝ICP备15012534号-6

>Copyright:Journal of Netshape Forming Engineering 2014 All Rights Reserved

>Postal Code: Phone:Fax: Email:

>    

渝公网安备 50010702501719号