文章摘要
赵月伟,帅美荣,楚志兵,等.焊管冷弯回弹曲线方程构建及工艺优化[J].精密成形工程,2022,14(7):98-105.
ZHAO Yue-wei,SHUAI Mei-rong,CHU Zhi-bing,et al.Construction of Springback Curve Equation and Process Optimization of Welded Pipe during Cold Bending[J].Journal of Netshape Forming Engineering,2022,14(7):98-105.
焊管冷弯回弹曲线方程构建及工艺优化
Construction of Springback Curve Equation and Process Optimization of Welded Pipe during Cold Bending
  
DOI:10.3969/j.issn.1674-6457.2022.07.014
中文关键词: 焊管冷弯  回弹解析  回弹方程构建  工艺优化
英文关键词: cold bending of welded pipe  springback analysis  construction of springback equation  optimization process
基金项目:国家自然科学基金(U1710113);常州市领军型创新人才引进培育项目(CQ20200042);山西省重点研发计划(201903D121043);山西省研究生教育改革研究课题(2020YJJG241)
作者单位
赵月伟 太原科技大学 重型机械教育部工程研究中心太原 030024 
帅美荣 太原科技大学 重型机械教育部工程研究中心太原 030024 
楚志兵 太原科技大学 重型机械教育部工程研究中心太原 030024 
桂海莲 太原科技大学 重型机械教育部工程研究中心太原 030024 
赵晓东 太原科技大学 重型机械教育部工程研究中心太原 030024 
高虹 武进不锈股份有限公司江苏 常州 213111 
邬莉华 中钢不锈钢管业科技山西有限公司太原 030600 
翟丽丽 武进不锈股份有限公司江苏 常州 213111 
摘要点击次数: 1647
全文下载次数: 904
中文摘要:
      目的 研究316L奥氏体不锈钢板材JCOE弯曲卸载回弹和应力分布特征,对预弯曲量实施相应补偿,以提高弯曲成形精度。方法 基于弹塑性变形理论,利用有限元模拟研究各关键成形参数对板材弯曲卸载回弹的影响规律,将影响指标线性/非线性拟合叠加,构建回弹曲线方程。结果 板料回弹量与上模下压量、下模开口量呈线性关系,与上模下行速度、摩擦因数呈指数关系。结论 优化后的最佳冷弯成形工艺参数如下:上模下压量为12 mm,下模开口量为150 mm,上模下行速度为4 mm/s,摩擦因数为0.15。对于径壁比值≤10的板料成形,理论计算得到的弯曲回弹量与实测平均值吻合较好,构建的模型可以为实际生产奠定理论基础。
英文摘要:
      The work aims to study the bending unloading springback and stress distribution characteristics of 316L austenitic stainless steel plate JCOE and impose corresponding compensation to pre-bending value, to improve the bending accuracy. Based on the elastic-plastic deformation theory, the effects of key forming parameters on plate bending and unloading springback were studied by finite element simulation method. The equation of springback curve was also established through linear/nonlinear fitting and superposition of affecting parameters. The springback had a linear relationship with the displacement of upper mold and the opening degree of lower mold, but had an exponential relationship with the speed of upper mold and the friction coefficient. The optimal parameters are as follow:the displacement of upper mold is 12 mm, the opening degree of lower mold is 150 mm, the speed of upper mold is 4 mm/s, and the friction coefficient is 0.15. The calculated bending springback value is in good agreement with the measured average value for the plate with diameter-wall ratio ≤10. The established model can provide a theoretical foundation for the practical production.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第13998036位访问者    渝ICP备15012534号-6

>版权所有:《精密成形工程》编辑部 2014 All Rights Reserved

>邮编:400039 电话:023-68679125传真:02368792396 Email: jmcxgc@163.com

>    

渝公网安备 50010702501719号