文章摘要
张小勇,程鹏志,王耀,等.三维异形截面管件充液成形工艺及优化分析[J].精密成形工程,2020,12(3):125-130.
ZHANG Xiao-yong,CHENG Peng-zhi,WANG Yao,et al.Hydroforming Process and Optimization Analysis of Three Dimensional Special Section Tube[J].Journal of Netshape Forming Engineering,2020,12(3):125-130.
三维异形截面管件充液成形工艺及优化分析
Hydroforming Process and Optimization Analysis of Three Dimensional Special Section Tube
投稿时间:2019-12-13  修订日期:2020-05-10
DOI:10.3969/j.issn.1674-6457.2020.03.015
中文关键词: 液压成形  三维异形截面  纵梁  高强钢  数值模拟
英文关键词: hydroforming  3D special section  longitudinal beam  high strength steel  numerical simulation
基金项目:江苏省基础研究计划(自然科学基金)青年基金(BK20160298);国家科技重大专项(SK201901A30-01);河北省自然科学基金青年基金(E2019202224)
作者单位
张小勇 1. 同济大学 汽车学院上海 200000 
程鹏志 2. 清华大学 苏州汽车研究院(相城)江苏 苏州 2151343. 航宇智造(北京)工程技术有限公司北京 1001914. 天津天汽模航宇高压成形技术有限公司 天津 300000 
王耀 4. 天津天汽模航宇高压成形技术有限公司 天津 3000005. 河北工业大学 机械工程学院天津 300401 
阮尚文 4. 天津天汽模航宇高压成形技术有限公司 天津 300000 
成刚 3. 航宇智造(北京)工程技术有限公司北京 100191 
王增华 3. 航宇智造(北京)工程技术有限公司北京 100191 
摘要点击次数: 3229
全文下载次数: 1955
中文摘要:
      目的 研究三维异形截面汽车纵梁充液成形过程的变形规律。方法 通过数值模拟和试验研究相结合的方法,分析多工序中的充液成形过程,对影响构件成形性能的液压力加载路径关键参数进行分析。结果 线性加载路径下试件最大减薄率为26.3%,试件出现了局部开裂现象。两段式线性加载条件下最大起皱指标为0.149,试件出现了起皱缺陷,最大壁厚减薄为23.2%,开裂现象并未明显缓解。分段式线性加载条件下试件的最大减薄率仅为16.8%,贴模偏移量为1.89 mm,未出现起皱叠料现象,成形质量较好,同时,试验结果与数值模拟结果有较好的一致性。结论 液压力加载路径对试件壁厚分布影响较大,采用分段式线性加载,可以实现低压阶段的分段加压和有效补料,以及后期的线性高压整形,试件成形质量较高。
英文摘要:
      The paper aims to study the deformation rule of three-dimensional special cross-section automobile longitudinal beam in hydroforming. Through the combination of numerical simulation and experimental research, the process of liquid filling forming in the multi process was analyzed, and the key parameters of the hydraulic pressure loading path that affected the forming performance of the components were analyzed. Combined with numerical analysis and test verification: under linear loading path, the maximum thinning rate of the specimen was 26.3%, and the specimen had local cracking; under two-stage linear loading condition, the maximum wrinkle index was 0.149, the specimen had wrinkle, the maximum wall thickness thinning was 23.2%, and the cracking phenomenon was alleviated obviously; under sectional linear loading condition, the maximum thinning rate of the specimen was only 16.8%, the offset was 1.89 mm, and the forming quality was good and free from wrinkle. At the same time, the experimental results were in good agreement with the numerical simulation results. The loading path of hydraulic pressure has a great influence on the wall thickness distribution of the test piece. The sectional linear loading can realize the sectional pressure and effective feeding in the low-pressure stage, and the linear high-pressure shaping in the later stage. The forming quality of the test piece is high.
查看全文   查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第14771333位访问者    渝ICP备15012534号-4

>版权所有:《精密成形工程》编辑部 2014 All Rights Reserved

>邮编:400039 电话:023-68679125传真:02368792396 Email: jmcxgc@163.com

    

渝公网安备 50010702501719号