崔长齐,闫绍国,林晨华,等.采用连铸连锻的技术防治合金铸件缺陷[J].精密成形工程,2013,5(4):69-73. CUI Chang-qi,YAN Shao-guo,LIN Chen-hua,et al.Solution to the Defect of Aluminium Alloy Foundry Goods by Continuous Casting and Forging Process[J].Journal of Netshape Forming Engineering,2013,5(4):69-73. |
采用连铸连锻的技术防治合金铸件缺陷 |
Solution to the Defect of Aluminium Alloy Foundry Goods by Continuous Casting and Forging Process |
投稿时间:2012-10-19 修订日期:2013-06-01 |
DOI:10.3969/j.issn.1674-6457.2013.04.018 |
中文关键词: 连铸连锻 铸造 缺陷 7 A04 铝合金 |
英文关键词: continuous casting and forging cast defect aluminum alloy 7A04 |
基金项目: |
|
摘要点击次数: 5120 |
全文下载次数: 4819 |
中文摘要: |
分析了 7 A04 铝合金铸造工艺中出现各种缺陷的成因,在现有生产设备的基础上提出采用连铸连锻工艺降低 7 A04 铝合金铸造缺陷出现的几率,验证了连铸连锻工艺的可行性,指出了采用连铸连锻工艺的注意事项。 |
英文摘要: |
This paper analyzes the cause of formation of defects in casting procedures of 7A04 aluminium alloy, suggests a technique of continuous casting and forging process based on the existing facilties, proves the feasibility and points out the precautions. |
查看全文
查看/发表评论 下载PDF阅读器 |
关闭 |
|
|
|